Zinc Oxide 99% active free sample
Zinc Oxide / ZnO Properties
Molecular formula |
ZnO |
Molar mass |
81.408 g/mol |
Appearance |
White solid |
Odor |
odorless |
Density |
5.606 g/cm3 |
Melting point |
1975 °C (decomposes)[1] |
Boiling point |
2360 °C |
Solubility in water |
0.16 mg/100 mL (30 °C) |
Band gap |
3.3 eV (direct) |
Refractive index (nD) |
2.0041 |
Zinc Oxide / ZnO Specification
Item/Parameter |
Standard |
Zinc Oxide % ≥ |
ZnO 99.5% |
ZnO 99.7% |
ZnO 99.8% |
ZnO 99.9% |
Metallic Zinc (in accordance with Zn) % |
None |
None |
None |
None |
Lead oxide (PbO)%≤ |
0.05 |
0.037 |
0.001 |
0.001 |
Cadmium oxide (CdO) % ≤ |
-- |
-- |
0.0005 |
0.0005 |
Cupric oxide (CuO) % ≤ |
0.0004 |
0.0002 |
0.0002 |
0.0002 |
As ≤ |
-- |
-- |
0.0005 |
0.0005 |
Manganese (Mn) % ≤ |
0.0001 |
0.0001 |
-- |
-- |
Ferro Oxide (FeO) % ≤ |
-- |
0.001 |
-- |
-- |
Muriatic Acid Insoluble Substance % ≤ |
0.008 |
0.006 |
0.004 |
0.004 |
Loss On Ignition % ≤ |
0.2 |
0.2 |
-- |
-- |
Water Insoluble Substance % ≤ |
0.2 |
0.1 |
-- |
-- |
Volatile 105°C % ≤ |
0.4 |
0.3 |
0.3 |
0.3 |
Sieve Residue (45um mesh ) % ≤ |
0.1 |
0.1 |
0.1 |
0.1 |
Surface Area % ≥ |
45 |
50 |
60 |
60 |
Oil Absorption g/100g ≤ |
-- |
14 |
-- |
-- |
Reducing Power (compared with standard sample) % ≥ |
-- |
100 |
-- |
-- |